[1] 李寿楠. 聚变-裂变混合堆——中国发展增殖堆的道路[J]. 物理,1987,16(8):487.
[2] Kai-ming Feng. Design description document for the Chinese helium cooled solid breeder (CH HCSB) test blanket module (Version II)[Z]. 2005.10.20.
[3] Vollath D,Wedemeyer H,Günther E. Improved method for fabrication of lithium silicates[J]. Journal of Nuclear Materials, 1985,133&134: 221.
[4] Chang C C, Wang C C, Kumta P N. Chemical synthesis and characterization of lithium orthosilicate (Li4SiO4)[J]. Materials and Design, 2001, 22: 617.
[5] Heriberto Pfeiffer, Pedro Bosch, Silvia Bulbulian. Synthesis of lithium silicates[J]. Journal of Nuclear Materials, 1998, 257: 309.
[6] Cruz D, Bulbulian S. Synthesis of lithium silicate tritium breeder powders by a modified combustion method[J]. Journal of Nuclear Materials, 2003, 312: 262.
[7] Kunihiko Tsunchiya, Hiroshi Kawamura, Katsuhiro Fuchinone, et al. Fabracation development and preliminary characterization of Li2TiO3 pebbles by wet process[J]. Journal of Nuclear Materials,1998,1985-1990: 258.
[8] Donne M D, Gunther E, Schumacher G, et al. Research and development work for the lithium orthosilicate pebbles for the Karlsruhe ceramic breeder blanket[J]. Journal of Nuclear Materials, 1991, 179-181:796-799.
[9] Pannhorst W, Geiler V, Rǎke G, et al. Production process of lithium orthosilicate pebble[A]. Proceedings 20th Symposium on Fusion Technology[C]. Marseille, France: 1998.
[10] Chu C Y, Bar K, Singh J B, et al. Relationship between fabrication parameters and structural characteristics of sintered lithium orthosilicate[R]. CONF-88-417-15, DE88 00935.
[11] Piazza G, Reimann J, Günther E, et al. Characterisation of ceramic breeder materials for the helium cooled pebble bed blanket[J]. Journal of Nuclear Materials, 2002, 307-311: 811.
[12] Wbreitung, Werle H. Experimantal evidence for tritium release-controlling processes in lithium silicates[J]. Journal of Nuclear Materials, 1991,179-181: 847.
[13] Abramenkovs, Tiliks J, Kizane G, et al. Basic study of influence of radiation of radiation defects on tritium release process for lithium silicates[J]. Journal of Nuclear Materials, 1997, 248: 116.
[14] Moritani K, Magari T, Moriyama H. Tritium release kinetics of lithium silicates with irradiation defects[J]. Fusion Engineering and design. 1998, 39-40: 675.
[15] Abramenkovs A. Thermoluminesence study of irradiation lithium orthosilicate[J]. Fusion Engineering and design, 1998, 39-40: 693.
[16] 王和义, 赵君科, 罗阳明. 制备γ-LiAlO2陶瓷芯块的工艺参数的研究[J]. 硅酸盐通报, 1994, 4: 13.
[17] Heyi Wang, Zhao Junke, Luo Yangmin. Fabrication of γ-LiAlO2 spherical ceramics by a planet-type rotation process[J]. Journal of Nuclear Materials. 1994, 208: 195.
[18] 王和义, 孙颖, 赵君科, 溶胶-凝胶法制备锆酸锂陶瓷微球[J]. 高技术通讯, 1997, 8: 53.
[19] 杨本福,万竟平,曹小华,等. 锂陶瓷γ-LiAlO2放氚行为研究[J]. 原子能科学技术, 1999, 33(5):441. |